项目性能 |
性能子项 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
基本性能 |
比重 |
nan |
ASTM D792 |
1.65 |
g/cm³ |
机械性能 |
弯曲模量 |
23℃, 0.00 mm, Injection Molded, Procedure A, Method I (3 point load), 0.00 mm, Type I, Secant |
ASTM D790 |
12700 |
MPa |
弯曲强度 |
23℃, 0.00 mm, Injection Molded, Method I (3 point load), Procedure A, 0.00 mm, Type I |
ASTM D790 |
305 |
MPa |
断裂点伸长率 |
23℃, 0.00 mm, Compression Molded, Type I |
ASTM D638 |
2.4 |
% |
拉伸模量 |
23°C |
ISO 527-2 |
14000 |
MPa |
拉伸应力 |
Break,23°C |
ISO 527-2 |
205 |
MPa |
拉伸应力 |
23°C |
ASTM D638 |
195 |
MPa |
拉伸伸长率 |
Break,23°C |
ASTM D638, ISO 527-2 |
2.4 |
% |
弯曲模量 |
23°C |
ASTM D790 |
12700 |
MPa |
弯曲强度 |
23°C |
ASTM D790 |
305 |
MPa |
Charpy无缺口冲击强度 |
23°C |
ISO 179/1eU |
65 |
kJ/m² |
Izod缺口冲击强度 |
-40°C |
ASTM D256 |
105 |
J/m |
Izod缺口冲击强度 |
23°C |
ASTM D256 |
110 |
J/m |
Izod无缺口冲击强度 |
23°C |
ASTM D4812 |
1180 |
J/m |
热性能 |
热畸变温度 |
1.8 MPa,未退火 |
ASTM D648, ISO 75-2/A |
235 |
°C |
熔融温度 |
DSC |
ISO 11357-3 |
247 |
°C |